Szukana fraza: [Abstract = "Masonry compressive strength is typically obtained by testing stack bonded prisms under compression normal to its bed joint. Use of micro\-fibres enhances the pre\-cracking behaviour of masonry by arresting cracks at micro\-scale in the post\-peak region. These efforts are necessary to ensure that CLC blocks become more accepted in the world of building materials and considered as a reliable option for providing low\-cost housing."]